4mm thickness they do however go upto 15mm but you wouldn’t need that, 4mm would suit. Pm me and I can send you over options and costs.
Locally it’s tilemaster level flex plus
I’d use a decoupling board which I’d adhere over the pipes (4mm board) then prime and 6mm flex compound unless you can make some good mm up with...
Fell down the cracks ?
Ooohhh what’s its strength, that’s interesting if it’s a wearable surface aswell as a deep fill to 60mm
Murexin fma30 is suitable
I’d ply just to be sure
There’s curing agents that can dry pumped sand/cement bases within 7 days without the need of dpm’s etc but needs to in the mix when pumped, find...
Let. Them crack on, will be up in no time
J2 flooring
J2 flooring natural timbers
For appearance and longevity M series by harvey Maria, it’s an outstanding LVT, if one costs £40 and the other costs £50, so £10 difference, for...
J2 flooring, where you based ?
I would opt for quick step personally and ensure temps don’t go crazy high
I’d use a MS flexible adhesive to bond the XPS down, then use the sane adhesive over the top of the XPS then use a product called uni board 4mm,...
Pm me, what you got
Yeah 27 degrees, however my assumption would be if it’s consistently at 32 degrees it’s not an issue, if it drops to 12 and goes back to 32 etc it...
Yeah pretty standard to be fair, see it loads where companies buy underlays and adhere it to insulation panels for floors or walls
Call a chap called gavin 07547456011
It’s the same underlay as flex pro, should be fine